Metric Units US Units   Text   
 
 

© Copyright 2013 Abbott Apps   Click for User's Manual
Typical Modulus Values
Modulus represents the strength of the web under tension.
Choose a Web, select the value and copy it.
Close this form and paste value into Modulus.
WebGPaMpsi
Acetate1.80.26
PC2.40.35
PE10.15
PET4.40.64
PMMA2.10.30
PP3.10.45
PVC2.80.41
Nylon 6 (PA)0.950.14
PI9.11.32
Board30.44
Bond1.80.26
Magazine10.15
LightWeightCoatedPaper5.50.80
MachineFinishedCoated5.70.83
NewsPrint40.58
FineCoatedPaper6.30.91
SuperCalendared7.91.15
Aluminium6910
Steel20029
Summary of Inputs and Outputs
Inputs
TensionForce on web in machine direction (N or lb)
MisalignmentOut of parallel alignment (µm or mil)
WidthWeb width (mm or in)
SpanDistance between two rollers (mm or in)
DiameterDiameter of Downstream Roller (mm or in)
WrapDegrees of contact with Downstream Roller (°)
Frict.Coef.Coefficient of friction at Downstream Roller
ThicknessWeb thickness (µm or mil)
Outputs
Slack EdgeYes/No to one edge slack
TD OffsetLateral web shift from misalignment
WrinklesNone, Soft Wrinkle, Hard Wrinkle