Typical Modulus Values
Modulus represents the strength of the web under tension.
Choose a Web, select the value and copy it.
Close this form and paste value into Modulus.
WebGPaMpsi
Acetate1.80.26
PC2.40.35
PE10.15
PET4.40.64
PMMA2.10.30
PP3.10.45
PVC2.80.41
Nylon 6 (PA)0.950.14
PI9.11.32
Board30.44
Bond1.80.26
Magazine10.15
LightWeightCoatedPaper5.50.80
MachineFinishedCoated5.70.83
NewsPrint40.58
FineCoatedPaper6.30.91
SuperCalendared7.91.15
Aluminium6910
Steel20029
Summary of Inputs and Outputs
Inputs
TensionForce on web in machine direction (kg or lb)
Mod.Modulus of the web (GPa or Mpsi)
ThicknessWeb thickness (µm or mil)
WidthWeb width (mm or in)
Outputs
Strain %The % by which each web is stretched
Rad. CurlRadius of the curl. Smaller=Worse